Temp - UP : 165
Temp - DOWN : 165
Duration : 30 min | 3 hours cooling
Preparation : 1x layer, 8cm each
Method : Mould frame, one load/pass
Mould sheets : sanded stainless
Post : Milling (sides) - 1500 RPM @ 80 facing head, 600mm/min